  • Item
    Analysis of quartz floatability using design of experiments.
    (2019) Matos, Vanderson Eney de; Peres, Antônio Eduardo Clark; Pereira, Carlos Alberto; Nogueira, Stephânia da Consolação Silva
    Quartz floatability in cationic reverse flotation depends on the suitable choice of surfactant type and the conditions under which they are applied. The design of experiments (DOE) allows the evaluation of process variables, in a structured and independent way, with statistical validation and a limited number of tests. Tests of microflotation of quartz, in the size range -150 +75 µm, using factorial design of experiments, showed that etherdiamine leads to higher level of quartz floatability than ethermonoamine, favored by increase in collector concentration, at the high level of pH tested (11.0). Floatability values above 90% were achieved with the use of 3 mg/L of ether diamine for both pH levels, while with ether monoamine the target was reached only at pH 11.
  • Item
    Kaolinite removal from bauxite by flotation.
    (2016) Rodrigues, Otávia Martins Silva; Peres, Antônio Eduardo Clark; Henriques, Andréia Bicalho; Amorim, Bárbara Gonçalves
    This paper presents a potential condition to separate kaolinite through flotation when it is present in bauxite ore. This research anticipates a Brazilian industry requirement, considering the tendency towards the need for aluminosilicates removal from bauxite ores, as has already occurred in China. Kaolinite is the most abundant aluminosilicate, and gibbsite is the main aluminum bearing mineral in Brazilian bauxite ores. The first step was a fundamental study involving microflotation experiments with pure samples of kaolinite and gibbsite. Ammonium quaternary salts and amines were used as the collector and corn starch as the depressant. In a fundamental study, the best conditions determined in the first step were evaluated for the flotation of kaolinite from bauxite ore using laboratory scale experiments. Tests with AQ142/starch (pH 10) and CTAB (pH 7) led to satisfactory results. In general, the highest values of alumina/silica mass ratio were obtained with AQ142/starch and the highest values of mass recovery and metallurgical recovery were achieved with CTAB.
  • Item
    Dispersion degree and zeta potential of hematite.
    (2016) Alexandrino, Júnia Soares; Peres, Antônio Eduardo Clark; Lopes, Gilmara Mendonça; Rodrigues, Otávia Martins Silva
    The dispersion degree of the mineral particles in the pulp is especially relevant regarding the performance of the cationic reverse flotation of iron ores. The gangue minerals should remain dispersed while hematite particles should be selectively flocculated. The present study addressed determinations of dispersion degree and zeta potential of hematite in the presence of different dispersants, classified as organic polymeric (natural and synthetic), organic monomeric, and inorganic. Special attention was paid to results achieved at pH 10, used in plant practice. For natural organic polymers, correlation was observed between the dispersion degree and the increase in the negative value of zeta potential. Some synthetic organic polymers enhance the dispersion of hematite particles despite not affecting significantly the zeta potential. Sodium silicates, irrespectively of the SiO2/Na2O ratio, at pH 10, did not impact significantly either the dispersion degree or the zeta potential.
  • Item
    Estado de dispersão de partículas de hematita em polpas na presença de reagentes.
    (2013) Alexandrino, Júnia Soares; Peres, Antônio Eduardo Clark; Rodrigues, Otávia Martins Silva; Lopes, Gilmara Mendonça
    Os minérios de ferro a serem explotados estão com teores do mineral de interesse muitos baixos. Com a diminuição desses teores, ocorre uma necessidade maior de moer o minério em granulometrias mais finas. Os óxidos e hidróxidos metálicos, tais como os óxidos de ferro, tornam-se carregados quando dispersos em meio aquoso. As alterações ocorridas na superfície de óxidos e a formação de interface eletricamente carregada entre as partículas e o meio aquoso são controladas pelo pH e força iônica da solução em que são dispersos. Esses fatores levam à necessidade de se estudar o efeito da dispersão nas etapas de flotação, espessamento e filtragem. Este trabalho, em escala de laboratório, visou contribuir para a melhor compreensão do tratamento de minérios de ferro abordando a dispersão de polpas de hematita na presença de reagentes dispersantes ou agregantes. Foram avaliados quatorze reagentes orgânicos e inorgânicos nos ensaios de dispersão. O estudo da dispersão da hematita sem adição de reagentes mostrou uma diminuição do grau de dispersão na faixa de pH de 6,5 a 7,5. As adições de amido e fubá levaram a agregação da hematita em toda faixa de pH, enquanto a dextrina levou ao aumento do grau de dispersão, na faixa alcalina. O tanino, reagente orgânico natural, que não agride o meio ambiente em caso de descarte, apresentou um aumento no grau de dispersão da hematita, mesmo em concentrações mais baixas (150 g/t). O ácido cítrico também levou ao aumento do grau de dispersão da hematita. A razão SiO2 /Na2O é um fator que pode interferir na ação do silicato de sódio na flotação do minério de ferro. O silicato de sódio C112, com razão mais baixa, não alterou significativamente o grau de dispersão; o silicato de sódio R3342, com maior razão, foi o que levou ao maior grau de dispersão. Já o silicato de sódio R2252 apresentou um aumento do grau de dispersão por volta de pH 8,5. O Dismulgan V3377 não mostrou muita diferença no grau de dispersão em todas as dosagens, mostrando certa semelhança com a curva de hematita pura. O Dispersogen LFS e o Polymax T10 levaram ao aumento do grau de dispersão na faixa alcalina de pH. O Bozefloc AE 738 pode ser sugerido como floculante. Em pH 10,5 apresentou uma boa agregação nas dosagens de 500g/t e 1000g/t. O reagente Dispersol 589 apresentou, em todas as dosagens estudadas, um aumento altamente significativo do grau de dispersão em toda faixa de pH. Em pH = 10,5, o reagente Depramin 158 levou a um aumento significativo do grau de dispersão. Na faixa ácida de pH, esse reagente levou a um grau de dispersão de aproximadamente 50%.
  • Item
    Kaolinite microflotation and zeta potential measurements in the presence of ammonium quaternary salts.
    (2010) Rodrigues, Otávia Martins Silva; Araujo, Armando Corrêa de; Peres, Antônio Eduardo Clark; Alexandrino, Júnia Soares; Lopes, Gilmara Mendonça
    Studies on kaolinite flotation are being driven by Chinese bauxite characteristics, presenting low alumina:silica weight ratios. This paper addresses the effect of the presence of cetyl pyridine chloride (CPC) and cetyl trimethyl ammonium bromide (CTAB) on kaolinite floatability and zeta potential. The reagents were dosed at three concentrations and the best floatability results were achieved at the highest concentration level (1x10-4 mol/L). Zeta potential determinations showed that both quaternary salts (CPC and CTAB) shift the kaolinite zeta potential to more positive values the specific collectors adsorption onto the mineral surface.
  • Item
    Recuperação de cobre por eletroeluição de resinas poliméricas de troca iônica a partir da reciclagem de placas de circuito impresso de computadores sucatados.
    (2013) Pereira, Carlos Alberto; Torem, Maurício Leonardo; Silva, Heloisa Regina Turatti; Peres, Antônio Eduardo Clark; Martins, Afonso Henriques
    Este trabalho apresenta os resultados para a recuperação de cobre presente em soluções aquosas sintéticas com concentração similar a de licores de lixiviação da reciclagem de computadores sucatados, através da técnica de eletroeluição de resina polimérica catiônica Amberlite IR-120®( Merck S.A., USA). A resina foi carregada pela passagem de 200 mL de solução aquosa 0,28 g/L de Cu em 2,18N H2SO4 através do leito de 10 g de resina. Os experimentos foram planejados com base em uma abordagem estatística pelo método fatorial de três variáveis a dois níveis experimentais. As condições consideradas estatisticamente ótimas visando a máxima eletrorrecuperação de cobre (96,56%) foram 150A/m2 de densidade de corrente catódica, com 100 rpm de intensidade de agitação do eletrólito e tempo de eletroeluição de 164 minutos. Esse resultado é superior ao encontrado por outras técnicas de recuperação de cobre a partir de soluções aquosas originadas de técnicas de reciclagem hidrometalúrgica de placas de circuito impresso de computadores sucatados, como por exemplo, precipitação de sais de cobre com 34,3% de recuperação.
  • Item
    Escolha ótica aplicada à pré-concentração de minério oxidado de zinco.
    (2012) Martins, Lemyr; Peres, Antônio Eduardo Clark; Galery, Roberto; Pereira, Carlos Alberto
    No depósito de zinco de Vazante o minério é silicatado, sendo a willemita o mineral-minério principal e a dolomita o principal mineral de ganga. O minério é retirado da mina subterrânea e enviado ao concentrador onde é submetido às etapas de britagem, moagem, flotação de zinco, flotação de carbonatos, espessamento e filtragem. Buscando aumentos no teor e recuperação de zinco e redução de contaminantes (carbonatos e magnésio) no concentrado foi investigada a préconcentração por escolha ótica. Os resultados, apresentados e discutidos neste trabalho, foram divergentes. Em algumas condições operacionais resultados muito bons foram obtidos, porém em outras condições o desempenho operacional foi pouco satisfatório.
  • Item
    Flotation routes for a phosphate ore bearing silicate-carbonate gangue.
    (2012) Albuquerque, Rodrigo Oscar de; Peres, Antônio Eduardo Clark; Aquino, José Aury de; Pereira, Carlos Alberto
    This laboratory scale investigation addressed two different process routes for the concentration of a phosphate ore bearing a silicate-carbonate gangue: (i) bulk apatite and calcite flotation followed by calcite flotation in the presence of phosphoric and citric acids; (ii) calcite flotation in the presence of carbon dioxide followed by apatite flotation. The target of selectively separating apatite from the contaminating silicates and carbonates was achieved. Following the flotation experiments, calcite zeta potential determinations were performed aiming at clarifying the mechanisms that rule the adsorption of the soybean bran oil soap onto the mineral surface in the presence of the modifying agents phosphoric acid, citric acid, and carbon dioxide.
  • Item
    Carbonate content reduction in zinc ore concentrate.
    (2012) Martins, Lemyr; Peres, Antônio Eduardo Clark; Galery, Roberto; Pereira, Carlos Alberto
    The hydrometallurgical zinc extraction from the willemite concentrate is impaired by the presence of high carbonate content. A stiff froth is produced causing zinc losses and acid consumption. A standard procedure was developed to de􀃀 ne the acceptable froth layer height in a laboratory test. Froth layers shorter than 2 cm resulted from carbonate content in the concentrate below 10.8%. The feasibility of adding a carbonate 􀃁 otation stage to the circuit was tested in laboratory and pilot scales. Among the collectors investigated, only those presenting a saponi􀃀 cation degree above 189 mg KOH/mg were effective in the laboratory experiments. Oleine and rice bran oil soaps were selected for the pilot scale experiments. The 􀃀 nal stage was a one month long industrial trial performed in a circuit consisting of three pneumatic cells G18. A comparison between the average results of the industrial trial including the carbonate 􀃁 otation stage and data of the raw industrial concentrate indicated that the MgO content in the concentrate dropped from 3.7%–3%. Concurrently, the carbonate content in the concentrate dropped from 11%–10.6%, the zinc grade in the concentrate increased from 41.4%–42% and the zinc recovery increased from 86.6%–89.8%. The concentrate was processed in the hydrometallurgical plant with no frothing problems.
  • Item
    Effects of hematite surface characteristics on filtration process.
    (2016) Graça, Leonardo Martins; Lagoeiro, Leonardo Evangelista; Galery, Roberto; Peres, Antônio Eduardo Clark
    In iron ore pelletizing plants a range of process parameters such as particle size distribution, specific surface area, and moisture, must be controlled to achieve opti¬mized operation conditions. Particle size distribution and specific surface area are con¬trolled during the grinding operations. Moisture, however, is controlled during filtra¬tion of the ground products. This work investigates the relationship between particle morphology, filter cake moisture and filter capacity. The samples were taken during the filtration tests and referred to three different blends presenting distinct mineralogical features and similar chemical compositions in order to investigate the effects of only the hematite surface characteristics. Six types of morphology are distinguished: granu¬lar hematite, tabular hematite, martitic hematite, polycrystalline hematite, hematite-goethite aggregates and goethite. For each filtration test, the filter cloth product was characterised. The characterisation analysis revealed that blends containing martitic hematite concentration above 11.45 percent increased substantially the filter capacity. However, it had also caused an increasing in final moisture content that reached values around 10.0 % compared with industrial moisture specification that can vary on the range of 8.5 to 9.5 %.